Integral skin System blended polyol
Home » Busniess » Applied Chemicals Series » Integral skin System blended polyol
Integral skin System blended polyol
Integral skin System blended polyol Integral skin System blended polyol
Integral skin System blended polyol Integral skin System blended polyol

loading

Integral skin System blended polyol

Availability:

A.Blended Polyol

ItemIndex
Material Temperature20~25℃
Mold Temperature40~50℃
Cream Time15~25s
Rising Time50~70s
POL/ ISO Ratio100:45~55

*The actual reactivity characteristics may be adjusted according to process conditions and clients’ requirements


B.ISO

BrandNCO%Details
Liquefied MDI29.5Liquefied MDI
JHW854529.9Modified MDI, good performance in integral skin